Wednesday, September 14, 2016

[MW:25389] RE: 25381] MAGNETISED AFTER OVERLAY

Electro slag weld overlay incorporates use of External Magnetic Field (Magnetic Oscillations).This is mandatory practice , for strips over 60mm width to prevent edge under cuts. Magnetic oscillations are done on a regular basis for electro slag weld overlays, without any residual magnetism in the welds.

 

Also it’s important to know what was the overlay material, Austenitic S.S, Nickel based alloys or Duplex stainless steel ?. If the it’s the first two then unless there is excess dilution causing high ferrite in the weld overlay, there would not be residual magnetism . However this is unlikely for ESSC ,where typically the dilution level 10% or below. If the overlay is Duplex Stainless Steel then it would be magnetic.

 

Appreciate if you could provide more details for better explanations, including the details for magnetic oscillations.

 

 

Thanks.

 

 

Pradip Goswami, P.Eng,IWE

Welding & Metallurgical Engineering Specialist ,

Ontario,Canada.

ca.linkedin.com/pub/pradip-goswami/5/985/299

pgoswami@quickclic.net

pradip.goswami@gmail.com

 

 

 

 

 

-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Ankit Gandhi
Sent: Tuesday, September 13, 2016 4:24 AM
To: Materials & Welding
Subject: [MW:25381] MAGNETISED AFTER OVERLAY

 

Dear sir,

 

Base Material P4

WOL by ESSC and SAW process.

After wol material is magnetised and not possible to weld.

Please inform to avoid these and what is solution for this?

 

Regards

Ankit Gandhi

Whatsapp-08879457665

 

--

http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

---

You received this message because you are subscribed to the Google Groups "Materials & Welding" group.

To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.

To post to this group, send email to materials-welding@googlegroups.com.

To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/af7c0d13-4103-4f35-94eb-053ad2193cd8%40googlegroups.com.

For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...