On Wednesday, 7 September 2016 15:42:06 UTC+5:30, Vadivel Mahadevan wrote:
> Dear Experts!!
>
>
> I am from a Valve industry. I am doing fabrication of a valve. After butt welding of two plates, can I carry out skin machining till the plate surface, so that welding is not seen..
>
>
> I follow ASME Sec.IX for welding qualification.
> What are the factors i am supposed to consider.
>
>
> Thanks and regards
> Vadivel. M
> 9843993317
Dear
You can do machining on seam bbut after machining you have to follow ndt requirement.
For your satisfaction and reduce rework you can carried out ndt before machining but after machining NDT is required.
ASME SEC. IX not restrict m/c.
Regards,
Ankit Gandhi
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/536f54af-8077-458c-b4d0-b6325c1b0da1%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment