Tuesday, December 3, 2013

Re: [MW:19432] Gas - Pipeline Test pressure

Test pressure 1.1 times of  design pressure




Sent from Samsung Mobile


-------- Original message --------
From: Pankaj Katke
Date:02/12/2013 6:48 PM (GMT+05:30)
To: materials-welding@googlegroups.com
Subject: [MW:19430] Gas - Pipeline Test pressure

Dear All,

can anybody help me to know what is a Pneumatic Test Pressure for the pipeline ( 8" & 10") 

Design code - ASME B 31.8
Design Pressure - 120 bar 


Thanks in advance.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...