Dear Pramodh:

European classification is more precise for structural steels.
ASME is not "known" as detailed as Euro-norms when it comes to structural steels. 
Of course, P-No./Gr-No. classification in ASME is still reliable and useful but my recommendation is not insisting on finding an equivalent grade for your material further than P-No (and/or group number) equivalents,especially if your application is offshore structures. 

You can see this with J or K grades which are not well-distinguished in ASME or versatility in impact test temperature requirements or weather resistant grades etc.    

Regards
Ramin Kondori
Sr. QA/QC Engineer
SINOPEC

r.kondori@petroyada.com
+98-2123592322
+98-9132150320



On Sat, Nov 30, 2013 at 11:08 AM, B.Jawahar - QC INSPECTOR <jawaharcb@gmail.com> wrote:
Dear Mr.Promodh,
Sorry for this very late reply.ASTM A283D Maybe Equivalent for this EN S275JR.
Kindly check and reply if it is right.
Regards,
Jawahar.

On Saturday, July 23, 2011 3:16:35 PM UTC+3, PRAMODH NAIR wrote:
Experts,
 
Could you please give me the equivalent ASTM material for EN S275JR with reference code document.
 
Regards
Pramodh

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...