Dear Sir,
I have to weld SA 516 Gr.70 (37mm Thk) Tube sheet to SA 516 Gr.70 (10 mm Thk) Shell as per below given weld details.
I have Qualified WPS of P1 to P1 material for 20 mm max. Base metal Thikness.
Now as per QW-202.4 Thicker member Thickness shall be within the range permitted by QW-451. My thicker member thickness is 37 mm.
Kindly pls explain me to can I use WPS yes or No with explanation.
Regards
Hemant H suthar
Asst. Manager QA/QC
Chemithon Engineers Pvt Ltd.
Khanvel-Kheradi Road. Silvassa, UT of DNH
Website: www.chemithon.co.in
Office Contact: 0260 2677889 / 2677036 , 37 Cell : 9712973092
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment