if the fiber elongation exceeds the specified limit PWHT is required, since in your case vessel is subjected to PWHT, you need not worry about it as the dished along with entire vessel will be heat treated.


On 30 November 2013 11:02, Pinaki Boxi <boxi.pinaki@gmail.com> wrote:
Respected sir,
Description of vessel:- 18097m length X 4.1m dia
Shell course thickness :- 24mm 
2:1 Elliptical Head thickness :- 28mm after forming it will be come 25mm
Material :- SA516 Gr70
Service :- Air
As per section VIII div-I UCS-79 reduction by cold forming the as rolled thickness is more than 10./. at any location where the extreme fiber elongation exceeds 5./.
PWHT is required.
But as per drawing it is on PWHT,
i am really confused regarding forming of 2:1 Elliptical Head PHWT.
So pls conformed me  2:1 Elliptical Head PHWT is required or not, if no so what base of section - VIII div-I it is not required, or PWHT is required what base of section - VIII div-I it is required,

 
--
Thanks & Regards
Pinaki Boxi.
Fujairah, AUE.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...