Re: [MW:19391] GUIDLINES FOR IBR SHOP APPROVAL

Hi Hemant
 
Regulation 4A of IBR prescribes the procedure for shop approval by IBR (For steel making industry). Please check the IBR link below.
 

You can approach a laisoning agency to deal with IBR effectively. They can help you out better for getting all the regulatory compliance requirements fulfilled and to communicate with IBR officials like dept director/director.
 
Regards
Hrishi

 
On Wed, Nov 27, 2013 at 1:40 PM, Prakash Gotimukul <gprakash31@gmail.com> wrote:
The article deals with REGISTRATION of Boilers but the query asked is registration of a Manufacturer.?
Mr Hemant,
Please give details of product to understand your requirement.


On Wed, Nov 27, 2013 at 9:31 AM, shaikh ahmed <ahmedmech77@gmail.com> wrote:
Dear Hemant,
 
Check the attached file related to IBR approval procedure.
 
thanks,
Ahmed
On Mon, Nov 25, 2013 at 11:15 AM, hemant <hsuthar@chemithon.co.in> wrote:

Dear  Sir,

We have to approve our workshop as per IBR regulation. I required some guidelines for approval. Our shop is ASME approved.

Can u pls help me & give me some basic knowledge for IBR approval.

 

 

Thanks,

HEMANT SUTHAR

09712973092

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.



--
Rgds
G.Prakash
Mob:+97150 6617824

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...