I have to qualify a WPS for A luminium welding. The informations are:
 
1- Material: 1050A  (SB209)
2- MIG Process
3- Filler metal: ER1100 (Diameter is 1.2mm)
4- Butweld joint, Thickness is 10.97mm
 
Please tell me what mechanical tests should i release for this speimen according to ASME IX.
 