[MW:19383] Inconel repair

Dear Experts,
 
Material : Inconel  ( Ni: 31-34 %, Cr: 19-21%, Nb 8 - 10%)
 
Opearting Temeprature:  840 deg.C
Pressure   :  20 bar
Fluid : Methane reformed gas
Service:  Non sour
 
The  header pipe is 10" and  weleded with 28 weldelets of  welded on the head pipe as branch connetions.  After almost 6 years of service, cracks are noticed almost on all the weld toes.
 
Initially these joints are welded by GTAW process by using ERNiCrCoMo-1.  No PWHT.
 
Now one of expert has advised to remove all cracks by grinding,followed by DP,  Then solution annealing at 1100-1150 deg C for 3 hours and welded by ER NiCrMo3 after solution annealing.
 
Please advise whether it is correct.
Can ER NiCrMo3  have resistance to 840 deg. C
 
Please give suggestions for repair
 
Regards
 
Venkat
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...