Most important issue for socket weld is gap between tube end with socket end should be 1.6 mm min
Eyup Tan
james gerald <gerry_tup@yahoo.com> yazdı:
If you weld small diameter and less thickness, TIG welding may be preferred.Thanks & RegardsJ.Gerald Jayakumar
00974-55835810
On Thursday, November 21, 2013 1:28 PM, Prabir Kumar Singh <prabirkumarsingh86@gmail.com> wrote:
Dear All
In socket welding of high pressure steam pipeline we have to weld by
SMAW . But our Client ask us, first pass of welding should be by TIG
welding. Then SMAW welding. Is TIG welding necessary in socket
welding. Please suggest with any code reference
With Regards:
Prabir Kumar Singh
--
Sent from Kaiten Mail. Please excuse my brevity.