[MW:19331] Re: Corrosion on Stainless Steel Vessel Weld

Dear Raju,

As per Photographs it seems that Corrosive material used for the fitup of Vessel and grinding done to remove the same. During grinding corrosive material spread near to weld.


Regards,

Israr Ahmed
+919930308261

On Wednesday, November 20, 2013 6:52:09 AM UTC+5:30, kalidindi raju wrote:
Dear Friends,
 
On a recent inspection of a Stainless Steel Vessel, there were some corrosive stains observed on near the weld.
Please refer to the pictures attached.
The stains indicate a leakage/flow behavior of the containment.
However, when observed visually there was no leakage of any liquid.
 
The vessel was in service since 2008.
Material of construction is Stainless Steel SS 316.
 
What could be the probable cause of this behavior?
Please share your views.
 
Regards,
Eswar Raju.
 
 
 
 

On Wednesday, November 20, 2013 6:52:09 AM UTC+5:30, kalidindi raju wrote:
Dear Friends,
 
On a recent inspection of a Stainless Steel Vessel, there were some corrosive stains observed on near the weld.
Please refer to the pictures attached.
The stains indicate a leakage/flow behavior of the containment.
However, when observed visually there was no leakage of any liquid.
 
The vessel was in service since 2008.
Material of construction is Stainless Steel SS 316.
 
What could be the probable cause of this behavior?
Please share your views.
 
Regards,
Eswar Raju.
 
 
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...