Hope that this is not phosphor brone alloy then why u choose ER CuSn1, u should have choosen ERCu. As Bathula said, use Helium, preheat to around 400degree celsius, cover with glass wool area other than jonit to avoid dispation of heat. 


On Fri, Nov 29, 2013 at 2:58 PM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
Use Helium as a shielding gas because, risk of oxide entrapment in the weld pool is greatly reduced
and provides deeper penetration.

Preheating of the base metal is typically required to maintain the base metal at welding temperatures
without preheating, the high thermal conductivity of copper results in excessive loss of heat away from the
weld zone.

On 29 November 2013 14:46, Avis <aviss2000@gmail.com> wrote:
Dear All,
 
Anybody having experience is copper welding.  If yes please share your difficultites, and also welder availablity for the welding.
 
The base materials is ASTM B42 UNS C12200 (Cu - 99.9%)

P. No. is 31, SFA  - A5.7, F. No. 31.

Filler Wire Class - ER Cu Sn 1

With regards,
S. Sivasubramanian, Kuwait.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...