Friday, November 29, 2013

[MW:19405] RE: 19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

The correction to these mistakes will appear as "errata" in the 2nd part of this article.
 
Thanks
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: pgoswami [mailto:pgoswami@quickclic.net]
Sent: Friday, November 29, 2013 7:34 AM
To: 'Raghuram Bathula'; 'Raghuram Bathula'
Cc: 'materials-welding@googlegroups.com'
Subject: FW: 19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

Mr... Bathula,
 
Thanks for your appreciation.Although we took enough care to write a good article, some editorial mistakes in the paper did occur. Other than those this paper (a review article) should be worth reading and enjoying.
 
Regards.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
 
 


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Raghuram Bathula
Sent: Friday, November 29, 2013 3:52 AM
To: Materials-Welding
Subject: [MW:19400] Duplex Stainless Steel: Metallurgy, engineering codes & welding practices

Congratulations Mr Pradip Goswami for the article in current issue of SSW

Duplex Stainless Steels (DSS) are extremely high grade engineering alloys combining good corrosion resistance with high strength and ease of fabrication. These steels are frequently used in the oil and gas industries both in upstream and downstream applications for assemblies such as pipe work systems, manifolds and risers. Furthermore, these are used in the petrochemical industry in the form of pipelines and pressure vessels. These steels are designed to provide better corrosion resistance, particularly chloride stress corrosion and chloride pitting corrosion, in addition to having a higher strength than standard austenitic stainless steels such as Type 304 or 316, enabling thinner sections to be used and providing significant cost benefits.

By Ramesh Bapat, Senior Principal Engineer, Foster Wheeler Upstream & Pradip Goswami, P. Eng., IWE, Welding and Metallurgical Specialist - Ontario, Canada

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...