this type of weld repair procedure is called as stelliteing.

Essential requirements: 1. WPS for same or equivalent grade of material.
                                   2. A good welder qualified for welding especially insitu welding.
                                   3. PQR
For Vinod : i have experienced same issue for one of my repair project on an Marine Boiler Superheater Valve having same material composition of SA 217 WC6.
You can use ECoCr-A welding electrode for welding (SFA - 5.13)
PWHT depending upon thickness.
 
Cheers,
Sharafat Dhanse.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...