RE: [MW:19379] Re: SEC-IX RT acceptance

Step back for a minute from the wording of QW-194.  Look at paragraph QW-144;  “Visual examination as described in QW-194 is used to determine that the final weld surfaces meet specified quality standards.”  Note that this paragraph does not state “as per Section IX” or “as per QW-XXX”.  It refers to “specified quality standards.”  In my opinion this statement is the result of Section IX being applied to/specified by numerous design Codes or other standards which modify requirements of Section IX.  Ultimately, the manufacturer  (ref. QW-103.1) is responsible for the quality of welding, as noted by Mr. Pieper.  Why an employer would accept welding of lessor quality of welding during the test phase than required for work to be performed is beyond my comprehension.  This is an invitation to disaster during production welding.  (Unless the guy is your cousin or brother-in-law.)

 

Further, looking at the wording of QW-194, what exactly do you interpret “complete fusion” to mean?  Excessive undercut, as defined in the applicable Code or your quality system, is in effect, incomplete fusion. 

 

I also think you need to consider that if one Code/Standard, referencing Sc IX, is more lenient than another is some regard, why would you tie a manufacturer producing equipment to the former, to comply with the more restrictive standard?  This lunacy has permeated the petro-chem industry and made fabrication of ordinary equipment (minimal service requirements) inordinately expensive and difficult. 

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kumar
Sent: Tuesday, November 26, 2013 3:19 AM
To: materials-welding
Subject: Re: [MW:19375] Re: SEC-IX RT acceptance

 

Agree mr. Joseph...but at the time of test the governing code is only sec.ix..then if the other party argue like this (sec.ix only want complete fusion and penetration),...then how to resolve ?..this is the issue..just for info...

On Nov 26, 2013 1:12 PM, "Roy Joseph" <royjoseph04@gmail.com> wrote:

Mr Kumar,

Other Sections of the Code may specify different requirements than those specified by Section IX and  Such requirements take precedence over those of  Section IX, and the manufacturer or contractor shall comply with them.

so 2mm undercut can not be accepted by any code.

 

On Tue, Nov 26, 2013 at 12:28 PM, Kumar <sk7920541@gmail.com> wrote:

Hai
Noted the responses from all and thanks..but still if project spec. Is silent and sec.ix doesnt have any ruling on other defects (porosity, sla g , under cuts, uf,etc..then a welder on test making 2mm u/c in test but then he passed and send to asme b 31.3 project where 1mm is the maximum u/c...that itself is contradicting...I feel sec.ix criterias must be strong where in most cases we rely on welders (random ndt)...please share ur opinions
Thanks in advance,
Kumar

On Nov 25, 2013 2:54 PM, "hpi001" <info@pieper-qsi.nl> wrote:

Dear Kumar,

 

Nothing mentioned in ASME Section IX regarding undercuts, under-fill etc.

Because ASME is based on manufacturers responsibility it would be the responsibility of the manufacturer to determine it's own requirements for this kind of defects, this can be classified as Good Workmanship.

In my opinion this should be discussed in front before start of production at a manufacturers workshop (for example during a kick-off meeting) in order to avoid any discussions afterwards.

 

Regards Herman Pieper

Op maandag 25 november 2013 08:21:52 UTC+1 schreef sunilkumar kundothara:

Dear All,

When conducting  WPQT(welder performance qualification test), the
acceptance criteria for both visual & RT is SEC.IX, but the these are
seemed to be much short & liberal. like,

Visual- complete fusion & penetration only required for visual, then
what about undercuts, underfill, re-inforcement height etc ?
RT- only chart given is for porosity comparison (attached herewith).
what about slags and other defects?

If anybody has more details of the above part of  SEC.IX, please share.
due to these reasons some times we find difficulty to judge sub-con
welder performances.
could we refert the construction code of the intended project in that case?
Appreciating your valuable feedbacks.
Thanks in advance,
Kumar

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...