Re: [MW:19344] RES: 19338] Chemical composition ASTM A234 Gr. WPB

Wen Cr + Mo is restricted to .32 hw can Cr alone be .40 max?

On Nov 23, 2013 9:25 AM, "MUNHOZ Sergio TECHINT" <tbrsmu@techint.com.br> wrote:

Follow my interpretation:

You can have 0.40% "Cr" individually without presence of "Mo"; by the other hand if you have "Cr" + "Mo" the sum cannot exceed .32.

 

regards

 

De: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] Em nome de PUB:José Luís Ferreira
Enviada em: sexta-feira, 22 de novembro de 2013 10:56
Para: materials-welding@googlegroups.com
Assunto: [MW:19338] Chemical composition ASTM A234 Gr. WPB

 

Please, 

 

I need solve a doubt about chemical composition of ASTM A234 Gr. WPB.

 

In the table 1 for grade WPB, for Cr is specified 0,40 max. and for Mo is specified 0,15 max., but in note F (The sum of Cr + Mo = 0,32 max.), how can be this? if for Cr is allowed until 0,40.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...