Dear Vijay,
On Wednesday, November 13, 2013 2:40:30 PM UTC+5:30, vijay wrote:
-- First of all you have to do stress re-leaving not normalizing, if you have done normalizing you have to put a test coupon to re verify mechanical properties.
Then You can do welding if You are going to do Stress Re leaving of full vessel.
If Dish end normalized and you are going to weld some nozzle on that stress will develop adjacent to weld that stress to be removed.
On Wednesday, November 13, 2013 2:40:30 PM UTC+5:30, vijay wrote:
Dear sir,
I have the following doubts to clear in the fabrication of CS plate 25thk
1. can i weld buildup in dish end after normalizing?
Please give your valuable advice
Thank You
BEST REGARDS
vijay kurkutiya
Get your own FREE website, FREE domain & FREE mobile app with Company email.Know More >
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments