Tuesday, November 26, 2013

Re: [MW:19384] WPS for Normalize plate and TMCP Plate

Dear Joanne,
 
Please refer to ISO 15608 & ISO 15614. Thermomechanically treated steels are grouped under group no. 2 and normalized steels are under sub group no. 1.3 under group no.1 in ISO 15608. If you have a WPS for welding between steels grouped under 2, ISO 15614 permits welding between the same group of steels or lower (i.e. 2 to 2, 2 to 1, 1 to 2). At the same time, it does not permit welding in the reverse (i.e. WPS for normalized will not be useful for welding of thermomechanically treated steels) as normalized steels are grouped under lower group.
 
Good Luck.
 
Megnath
 
 
----- Original Message -----
From: Joanne Wai
Sent: Tuesday, November 26, 2013 11:43 AM
Subject: [MW:19370] WPS for Normalize plate and TMCP Plate

Is there any rules that states that WPS qualified with TMCP plate cannot be used for normalized plate and vice versa?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...