Re: [MW:15725] Minimum spots of hardness in a pipe weld.

Dear Hareesh,
Normally we have taken the hardness in the order of PM,HAZ,WELD,HAZ,PM. If the pipe is less than 12", we can take 2 spots like 0 and 180 degrees. 4 spots for 12"  and over. Average of three spots in each spot (For example in 0 degree three spots  in every PM,HAZ,W,HAZ,PM) shall be taken for consideration. There is a setting also in the hardness machine. Refer your hardness test procedure which is approved by your client or get help from your NDE contractor. 

Muthusamy.S


On 20 October 2012 13:27, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir's,

What is the minimum number of spots to be taken for hardness in a pipe
weld. Some clients are specifying to take 3 or 4 spots and take the
average. Any code references. My construction code is ASME B31.3. But
if it there in any other construction code also, it will be helpfull
for me.

Please share your experience.

Thanking You,

----------------------
Hareesh K V
+91-9447625012

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...