Re: [MW:15741] Minimum spots of hardness in a pipe weld.

Dear Hareesh,
 
You can Use ASTM A833 for procedure, you have to take weld and HAZ, normally we should take at the bottom od the welding and at the top of the welding.

On Sat, Oct 20, 2012 at 12:27 PM, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir's,

What is the minimum number of spots to be taken for hardness in a pipe
weld. Some clients are specifying to take 3 or 4 spots and take the
average. Any code references. My construction code is ASME B31.3. But
if it there in any other construction code also, it will be helpfull
for me.

Please share your experience.

Thanking You,

----------------------
Hareesh K V
+91-9447625012

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
Thanks & Regards
Biplab Pal
Welding Inspector
E-mail:   biplab.mech@gmail.com
 
Information in this email and any attachments is confidential and intended solely for the use of the individual(s) to whom it is addressed or otherwise directed. Please note that any views or opinions presented in this email are solely those of the author and do not necessarily represent those of the Company. Finally, the recipient should check this email and any attachments for the presence of viruses. Myself accepts no liability for any damage caused by any virus transmitted by this email.
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...