Dear experts please clarify the below matter,
Our vessel is of cladded(ie. CS & SS 316L). To perform PWHT for such
vessel by internal oil firing is it acceptable or not . If it is
acceptable or not then whats the effect on ss to prevent from
corrosion during service. Please clarify this matter in detail.

With warm regards
Krishna M.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...