Dear all,
T-274.1 Geometric Unsharpness Determination.
Geometric unsharpness of the radiograph shall be determined in accordance with:
U
g = Fd/D
where,
U
g = geometric unsharpness
F =
source size: the maximum projected dimension of the radiating source (or effective focal spot) in the plane perpendicular to the distance D from the weld or object beingradiographed
D =
distance from source of radiation to weld or object being radiographed d p distance from source side of weld or object being radiographed to the film D and d shall be determinedat the approximate center of the area of interest.
Please refer Sec -V ASME for more details.
Thank & Best Regards,
M Veera SAMY- Bureau Veritas.
Coimbatore
Date: Tue, 30 Oct 2012 09:39:55 +0530
Subject: [MW:15801] Can we measure the Ug
From: nagarajanqc187@gmail.com
To: materials-welding@googlegroups.com
Dear Experts,
Can we measure the Ug in RT interpretitation ? If Yes , How to measure tell me
with regaeds
nagu
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments