Saturday, October 20, 2012

Re: [MW:15734] Minimum spots of hardness in a pipe weld.

Hi

Minimum number of spots 3, One each from weld, HAZ and base metal. More details available in BS 1043-1.

Regards,
Tomy George

On Sat, Oct 20, 2012 at 10:27 AM, HAREESH K V <hareesh13h@gmail.com> wrote:
Dear Sir's,

What is the minimum number of spots to be taken for hardness in a pipe
weld. Some clients are specifying to take 3 or 4 spots and take the
average. Any code references. My construction code is ASME B31.3. But
if it there in any other construction code also, it will be helpfull
for me.

Please share your experience.

Thanking You,

----------------------
Hareesh K V
+91-9447625012

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...