Fillet weld measurements
L: Leg length, S: Fillet weld Size, T: Theoretical throat,
V: Convexity, C: Concavity, W: Effective weld length



The strength of a fillet weld is based, in the design, on
the product (effective area of the weld: T ,W) of the
theoretical throat (design throat thickness) and effective
weld length as shown in. Fillet weld legs
determine fillet weld sizes. Fillet weld sizes are
measured by the length of the legs of the largest right
triangle that may be inscribed within the fillet weld
cross section.


Fillet weld sizes determine theoretical throat. The
product of the size and cos45􀋃in case where an isosceles
right triangle may inscribe within the fillet weld cross
section: S􀊷cos45􀋃= 0.7S, as shown in






WITH REGARDS
VICTOR KULKARNI
TEXAS,USA


On Sat, Oct 20, 2012 at 3:37 PM, Kishore Maharana <kishoremaharana@gmail.com> wrote:
Dear All
           Please suggest with proper standards calculation for fillet leg length and throat thickness calculation


Regards

Kishore

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...