Hi,

you cannot keep T/S blank in wps, since it is an essential variable in AWS D1.1, eventhough the impact test is not applicable.


Please check with your client, whether that structure frames is for low temperature service ?

Because, if impact test is required, then the CVN table for essential variables and supplementaries as per section 4 in AWS D1.1 all to be recorded and to be used, during PQR and for making WPS.

You should have recorded T/S during PQR, even for NO impact test condition.

With best regards,
Saravanan,
Korea





On Fri, Oct 26, 2012 at 3:39 PM, pradeep kumar <pradeepjayam@gmail.com> wrote:
Hi all,
 
We have a PQR qualified without impact test (as per AWS D1.1). Our project requirement says "Travel speed and Heat input shall be recored during procedure test". Does this says impact test is mandatory?
TPI told me to keep t/s and Heat input columns blank in WPS from that PQR -otherwise it means impact is mandatory.
Please help - how can I know if impact is mandatory or not if not mentioned in Construction code.
 
PS: WPS is for structural frames.
 
Thanks in advance
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...