Re: [MW:15792] Weld Defect Photos with Chinese Sub-Titles

you can collect defect photos as well as  good and mark like below and show them. try once.
好 = good.
坏  = bad

On Sun, Oct 28, 2012 at 6:34 AM, raj susi <rjsusi@yahoo.com.sg> wrote:

Dear friends
In my company (in Singapore)we have a lot of chinese welders and its difficult for me to explain the welddefects in chinese because they don understand english well.i have these  photos wit english titles,so if anyone has these photos with english and chinese titles please forward me so that I can display on our notice board and ask them to follow.
Thanks
Raj

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.





--
ELAVARASAN ARUMUGAM
GULF TURRETS
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...