Mr. Kishore,

Please suggest with proper standards calculation for fillet leg length and throat thickness calculation


With reference to above the calculations as follows:

1. Fillet leg length    ' L' - 0.75 times of Base Metal Thickness  (for load bearing structures)

2. Fillet leg length    ' L' - 0.38 times of Base Metal Thickness  (for non load bearing structures)

3. Throat thickness  ' t'  - 0.71 times Leg length.' L'

Hope it  will be of use to U.

Sridhar.
----------------------------------------------------------------------------------------------------------------------------------------------------------------