Dear experts,
we are doing welding in a vessel of joint nozzle to dish with reinforcement pad(pipe thick 10mm(32inch), dish thik 20mm & RF pad 20mm) the weld detail in drawing shows bevel(55 degree) followed with fillet(10mm). All are P1 material.
In my question : the total weld metal deposit is 50mm in a joint(40mm CJP & 10 Fillet)
code says above 38mm groove weld for P1 material PWHT is mandatory and also says groove & fillet exceed 26mm in 2inch pipe PWHT is required.
Now we will do PWHT or not in a particular joint. If not kindly tell the reason.
Regards
venkat
welding engineer
trichy.
----------
Sent from my Nokia phone
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
we are doing welding in a vessel of joint nozzle to dish with reinforcement pad(pipe thick 10mm(32inch), dish thik 20mm & RF pad 20mm) the weld detail in drawing shows bevel(55 degree) followed with fillet(10mm). All are P1 material.
In my question : the total weld metal deposit is 50mm in a joint(40mm CJP & 10 Fillet)
code says above 38mm groove weld for P1 material PWHT is mandatory and also says groove & fillet exceed 26mm in 2inch pipe PWHT is required.
Now we will do PWHT or not in a particular joint. If not kindly tell the reason.
Regards
venkat
welding engineer
trichy.
----------
Sent from my Nokia phone
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments