Hi Pradip,
UNS 31254 is a super austenitic stainless steel, popularly known as 254SMO.
See the attached document (highlighted texts) for instructions on welding ,
between similar base metals and dissimilar welds between C.S # UNS S31254.
For welds involving PWHT advisable would be to butter the C.S, perform PWHT
followed by welding to UNS S 31254.
Thanks
P.Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net
-----Original Message-----
From: pradip kumar sil [mailto:pradipsil@gmail.com]
Sent: Monday, October 29, 2012 3:40 AM
To: materials-welding
Cc: pgoswami
Subject: Dissimilar welding CS to DUPLEX SS
Dear Experts,
In our isometric drawing shows dissimilar welding carbon steel to duplex
stainless steel ( 31254 grade ) thk is 9.52 mm. Can anybody give me
guideline to make this WPS.
Regards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
UNS 31254 is a super austenitic stainless steel, popularly known as 254SMO.
See the attached document (highlighted texts) for instructions on welding ,
between similar base metals and dissimilar welds between C.S # UNS S31254.
For welds involving PWHT advisable would be to butter the C.S, perform PWHT
followed by welding to UNS S 31254.
Thanks
P.Goswami,P.Eng.IWE
Welding & Metallurgical Specialist
Ontario, Canada.
Email-pgoswami@sympatico.ca,
pgoswami@quickclic.net
-----Original Message-----
From: pradip kumar sil [mailto:pradipsil@gmail.com]
Sent: Monday, October 29, 2012 3:40 AM
To: materials-welding
Cc: pgoswami
Subject: Dissimilar welding CS to DUPLEX SS
Dear Experts,
In our isometric drawing shows dissimilar welding carbon steel to duplex
stainless steel ( 31254 grade ) thk is 9.52 mm. Can anybody give me
guideline to make this WPS.
Regards
Pradip
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments