Hi all,
 
We have a PQR qualified without impact test (as per AWS D1.1). Our project requirement says "Travel speed and Heat input shall be recored during procedure test". Does this says impact test is mandatory?
TPI told me to keep t/s and Heat input columns blank in WPS from that PQR -otherwise it means impact is mandatory.
Please help - how can I know if impact is mandatory or not if not mentioned in Construction code.
 
PS: WPS is for structural frames.
 
Thanks in advance
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...