Re: [MW:15749] welding LTCS CLADDED WITH B423 UNS N08825 using E7018-1

NO. You need to re qualify the WPS, as the F no is different.

Respectfully,

Nandesh Kumar A


--- On Tue, 9/10/12, Mohamed Elsayed ( BTG) <MElsayed@ccc.ae> wrote:

From: Mohamed Elsayed ( BTG) <MElsayed@ccc.ae>
Subject: [MW:15508] welding LTCS CLADDED WITH B423 UNS N08825 using E7018-1
To: materials-welding@googlegroups.com
Date: Tuesday, 9 October, 2012, 9:42 AM

Dear Experts,

 

   We have material LTCS CLADDED WITH B423 UNS N08825  and have approved WPS and PQR using Filler ERNICRMO-3 for GTAW in Root and Hot Pass and electrode ENICRMO-3  for SMAW in  Filling and Cap.

 

so, the question is , can be used another supporting PQR For CARBON STEEL (using Filler ER70S-3 in Root and Hot Pass and electrode E7018-1  for Filling and Cap )to produce WPS using Filler ERNICRMO-3 in Root and Hot Pass and electrode E7018-1  for Filling and Cap, due to shortage in ENICRMO-3.          

Any troubles may be happened regarding dilution or what

 

Waiting your scientific  and specific reply.

 

Thanks

Mohamed

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...