Friday, July 29, 2011

Re: [MW:11981] gas purging

Dear Prasad
Gas purging is done only on P number 5 and above base metal , purging is not based on welding process or type.
 
I hope the answer to your  question.
 
Regards
ABDUL JABBAR KHAN

--- On Fri, 29/7/11, Prasu Cutie <pracuty@gmail.com> wrote:

From: Prasu Cutie <pracuty@gmail.com>
Subject: [MW:11977] gas purging
To: materials-welding@googlegroups.com
Date: Friday, 29 July, 2011, 5:01 PM

Why gas purging is not mandatory for MIG welding as it is mostly used for TIG welding?

In MIG welding i found contamination is very lass as compared to TIG welding without purging.

Can any one clarify me??????


Regards
Prasad


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...