Power Intensity varies thats why votages varies.. 

GTAW is high intensity so voltage is less 

SMAW is less intensity welding process so required a bit high votlage,more over melting rate is very high in case of SMAW ,since electrode flux high voltage is required .

On Fri, Jul 29, 2011 at 5:06 PM, Prasu Cutie <pracuty@gmail.com> wrote:
Dear Experts,

for the same current voltages are different for GTAW & SMAW why???  Plz explain

GTAW     90-180A   9-14V


SMAW    90-180A   22-26V


Regards
Prasad

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With regards,
Sudhakar.k

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...