Friday, July 29, 2011

Re: [MW:11979] DOT/DWT qualification

No, you can use two or more qualified  welders to make a weld.
PQR is to test the soundness of the weld, doesnt take into acconunt who make it.



De:        Prasu Cutie <pracuty@gmail.com>
Para:        materials-welding@googlegroups.com
Fecha:        29/07/2011 10:24
Asunto:        [MW:11976] DOT/DWT qualification
Enviado por:        materials-welding@googlegroups.com




Dear Experts,
Is welder qualification & PQR qualification is required for DOT/DWT technique????? *(As per Sec.IX)

DOT-- Double operator technique
DWT-- Double welder technique

Awaiting for reply!!!!!!!!!

Regards
prasu

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

__________________________________________________________________ La información contenida en este mensaje es confidencial, y puede ser usada exclusivamente por aquellas personas a las cuales está dirigida, dentro de los límites establecidos para  su uso. Si este mail es recibido por error, agradeceremos a su receptor tenga a bien informar  esa circunstancia al emisor, dirigiendo el mensaje a la dirección de correo electrónico que lo haya remitido. En tal hipótesis, además, se solicita no copie ni revele el mensaje, como  así tampoco divulgue su contenido a terceras partes, para evitar un eventual comportamiento  ilícito. Las opiniones contenidas en este mensaje son exclusivas de su emisor y no representan  necesariamente la opinión de la empresa.  The information contained in this message is confidential, and is intended exclusively for the  individuals who have been specifically addressed, considering the limitations established for  its use. If this mail is received by error, please inform the sender and return the message  to the email address that had sent it. In such case, please do not copy or disclose the  message or its contents to any third party in order to avoid any unlawful conduct. The statements  included in this message belong only to the sender and do not necessarily constitute the  company s view.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...