www.t-put.com/EN_welding_CrMo.pdf
The above link is a good guideline for welding Cr-Mo steels. In page 3, figure 2 (left) demonstrates a good temperature cycle and heat control during welding and PWHT of martensitic P91 & P92 steel...
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
The above link is a good guideline for welding Cr-Mo steels. In page 3, figure 2 (left) demonstrates a good temperature cycle and heat control during welding and PWHT of martensitic P91 & P92 steel...
Ramin Kondori
QC/Welding Engineer
IWE AT 0070
On Wed, Jul 27, 2011 at 7:13 PM, Izhar Mustafa <izharmustafa@gmail.com> wrote:
Use ER90S-B9/E 9015-B9 welding consumable and use Induction method for pre-heat or Interpass temperature maintenance,,Set minimum 200C temperature and After welding do Intermediate post weld heat treatment. i.e after welding keep temperature minimum 250C and hold it minimum 1hour then cool down by 75C/h then allow free cooling under insulation.Hope for the best,,,,WishesIzhar.On Wed, Jul 27, 2011 at 7:14 PM, sudhakar kuppuswamy <mechsudhakar@gmail.com> wrote:
dear all,
please share your experience in repair welding of P91 or P92 ? please post your valuable welding tips like preheating techniques,filler metals that can be used for repair & so on !!!--
With regards,
Sudhakar.k
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments