This is how pressure could be applied from the Quality Assurance perspective:
There is a much higher risk of stray arcs on components from this type of electrode holder. This is a serious issue. The localized quenched and brittle microstructure that is left behind after a stray arc has been removed has serious design implications especially in a cyclic setting.
When one stray arc is found on a pressure retaining component (you will find many I assure you once you start looking) initiate a "Non-Conformance Report". In my jurisdiction, this "Non-Conformance Report" requires the determination of a root cause and a "Corrective Action" by the parties found to be at blame. Determine that the stray arc has been caused by this type of holder. The "Corrective Action" must be to use Electrode Holders from an approved list, with verifiable documentation to support the site-wide implementation of the new electrode holders.
So, as a Customer/Owner, the "Corrective Action" proposed by the Contractor must meet my approval (as the Owner's Inspector) in order to close the "Non-Conformance Report". I imagine there may be some similar Procedures in place in your jurisdiction??
Hope this helps,
Darcy
-----Original Message-----
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of lakshman kumar
Sent: Thursday, July 28, 2011 5:00 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:11964] SMAW - Welding Electrode Holder
Hi,
I do accept that this type of holders are not fit for use and will not give proper out put.
However just keeping this matter to open discussion - what are the laggings / shortfall / lapses with this type of holders.
Thanks and Regards.................
Lakshman Kumar.B|Manager- QA/QC |Lanco Infratech Limited Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004 Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com Go Green|The future will thank you Please note that my "Lanco group" mail is not working properly at some times, request you keep a copy to personal mail ID lakshmankumar4@gmail.com
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of jaya anil
Sent: Thursday, July 28, 2011 3:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11962] SMAW - Welding Electrode Holder
Dear Ashish,
In your case , I want to give one sugesstion, Go for Calibration of Welding machine along with Holder and other accesories. Prepare one Check list for Safety department for Welding Machine holder and other accesories. Make them to offer the same for Calibration Inspection and ask your Safety person to fulfill the check list, What ever is not safe your safety personal should ask them to replace or wind up the Machine with Red tag (Not to be used).
this is the one solution for people who dont want to follow Good Engineering practise.
Make a System ,Implement, Remove all unnessary items. (will be proper channel to solve your problem).
Link up Electrode Holder with Welding Machine.
On Thu, Jul 28, 2011 at 8:58 AM, Ash_Ish Soni <ashishsoni18@gmail.com>
wrote:
> Dear Member,
> I have come across to know that our contractor is using Welding
> Electrode Holder as per the attached photo. Contractor is big enough
> to force
without
> standard, so, I am searching for any International Standard which
> helps to force them to replace this kind of Welding Electrode Holder
> with the Standard one, which all of you know.
> I have come to know one standard - IEC - 60974 - 11, but that is only
> for Safety point of view, which is not enough.
> Request for the help.
> Thanks & Regards,
> Ashish Soni.
> Essar.
>
> --
> To post to this group, send email to
> materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views
> and meant for educational purposes only, Users must take their own
> decisions w.r.t. applicable code/standard/contract documents.
>
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments