Hi,

I do accept that this type of holders are not fit for use and will not give
proper out put.

However just keeping this matter to open discussion - what are the laggings
/ shortfall / lapses with this type of holders.

Thanks and Regards.................

Lakshman Kumar.B|Manager- QA/QC |Lanco Infratech Limited
Plot No 1255 | Sanjeevani chowk | Mahanadi vihar | Cuttack 753004
Phone : + 91 671 2445033 | Mobile : +91 9937286851 |www.lancogroup.com
Go Green|The future will thank you
Please note that my "Lanco group" mail is not working properly at some
times, request you keep a copy to personal mail ID lakshmankumar4@gmail.com

-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of jaya anil
Sent: Thursday, July 28, 2011 3:58 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:11962] SMAW - Welding Electrode Holder

Dear Ashish,

In your case , I want to give one sugesstion, Go for Calibration of
Welding machine along with Holder and other accesories. Prepare one
Check list for Safety department for Welding Machine holder and other
accesories. Make them to offer the same for Calibration Inspection and
ask your Safety person to fulfill the check list, What ever is not
safe your safety personal should ask them to replace or wind up the
Machine with Red tag (Not to be used).

this is the one solution for people who dont want to follow Good
Engineering practise.

Make a System ,Implement, Remove all unnessary items. (will be proper
channel to solve your problem).

Link up Electrode Holder with Welding Machine.

On Thu, Jul 28, 2011 at 8:58 AM, Ash_Ish Soni <ashishsoni18@gmail.com>
wrote:
> Dear Member,
> I have come across to know that our contractor is using Welding Electrode
> Holder as per the attached photo. Contractor is big enough to force
without
> standard, so, I am searching for any International Standard which helps to
> force them to replace this kind of Welding Electrode Holder with the
> Standard one, which all of you know.
> I have come to know one standard - IEC - 60974 - 11, but that is only for
> Safety point of view, which is not enough.
> Request for the help.
> Thanks & Regards,
> Ashish Soni.
> Essar.
>
> --
> To post to this group, send email to materials-welding@googlegroups.com
> To unsubscribe from this group, send email to
> materials-welding+unsubscribe@googlegroups.com
> For more options, visit this group's bolg at
> http://materials-welding.blogspot.com/
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to
materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and
meant for educational purposes only, Users must take their own decisions
w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...