WPS B is also accepted, if the deposited weld metal of a A106 Gr B pipe 4" sch 40 (GTAW process) is 2 (two) times from deposited GTAW in PQR B. the thing that you need is just re-write your welding procedure.

rgds,

2011/7/26 Dinesh Somwanshi <som.din@gmail.com>
you can use WPS A , as thickness & diameter range within an range & requirements.

regards

dinesh




On Tue, Jul 26, 2011 at 8:11 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
no restriction, you can use as there is no diamter restriction for procedure qualification in ASME.


On Tue, Jul 26, 2011 at 6:13 AM, Candice Law <candice.law@penergy.com.my> wrote:

 

Expert,

I have a 2 WPS qualified range as below:

1)     WPS A – Qualified Thickness Range from 1.6mm – 11.08mm ; diameter range is all diameter. (Gtaw process)

2)     WPS B – Qualified Thickness Range from 4.8mm – 22.0mm ; diameter range is all diameter. (Gtaw + Smaw process)

Both are qualified under ASME IX and for material with P No.1

 

Now, I need to weld a A106 GrB pipe 4" Sch40, can I use WPS A? Full Gtaw for 4" pipe? Any restriction for welding process pertaining diameter as in ASME IX?

 

Please Advice.

 

Thanks

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...