Re: [MW:11933] PQR qualified on TP-321 for welding TP-304L

yes , you can

On Tue, Jul 26, 2011 at 11:50 AM, pradip kumar sil <pradipsil@gmail.com> wrote:
> Hi,
> I have one wps with established pqr @ ASTM A-312 TP321H with filler ER-347.
> Can i establish ASTM - A-312 TP-304L with ER-308L with the help of
> ASTM-A-312 TP 321 PQR. Base metal & filler P no, Fno, SFA no, A,no & GROUP
> no & other variable are same.
> Can i use TP-321 PQR FOR establish of TP-304L.
> Waiting for ur valued reply.
> Regards
> Pradip
>

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS