Hi Srinivas,

Thanks, Can u tel r u using these machines, which model? What is repair percentage in RT? what are the major factor for good Orbital machines to get low repair rate, How u r achieving proper fit-up for Orbital welding as i know main factor of orbital welding is proper and accurate fit-up.


Regards

Izhar


On Mon, Jul 25, 2011 at 1:13 PM, Srinivas <srinivassirigineedi@gmail.com> wrote:

AMI MACHINES, good performance but costly

Cheers,
Srinivas
Sent from my iPhone 4

On 24-Jul-2011, at 8:03 PM, Izhar Mustafa <izharmustafa@gmail.com> wrote:

Dear Experts,

Can anyone have experience of Orbital welding GTAW from 2" to 14". Pl share practical experience with Machine info.
Will be thankful.

Regards

Izhar 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...