Re: [MW:11915] Pnumber of A 335 P92, P23

These are Unassigned material, we have to qualify seperately.

S.Eswaran

From: kannayeram gnanapandithan <kgpandithan@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, 24 July 2011 10:41 PM
Subject: Re: [MW:11891] Pnumber of A 335 P92, P23

P nos not yet assigned
pandithan

On Sat, Jul 23, 2011 at 1:46 PM, Sundar Rajan <as_sundarrajan@yahoo.com> wrote:
Dear all,
can anyone tell me that what is a P-number of A 335 P92, A335 P23 material. this is not given in QW-422 of ASME section 9. 
 
With Regards,
s.sundarrajan.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...