Re: [MW:12010] FILLET WELD QUALIFICATION BY BUTT WELD AS PER API 1104

yes ,consider the position also.

regards


On Sun, Jul 31, 2011 at 4:26 PM, Mahmoud <mqreis@gmail.com> wrote:
Yes

Regards
Mahmoud Qreis

On Jul 31, 2011, at 12:39 PM, "NAJM UL ISLAM" <najmislam246@gmail.com> wrote:

Dear Experts,

Greetings,

 

Can somebody advise me that if a welder is qualified for butt weld either in 5G position (Pipe horizontal) or 2G position (Pipe Vertical) whether  he will be qualified for fillet welds or not.

 

Thanks & Regards

 

NAJM UL ISLAM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...