Thursday, July 28, 2011

[MW:11966] Regarding plate welding of unlimited thickness

Dear Experts ,
 
If the wleder is  qualifide for 6G test , can he weld the plate of  unlimited thickness ?
or he needs to Qualify 4G test to weld unlimited thickness of plate ?
 
wether the 6G welder is sapose to weld only pipes.
 

awaiting for  welding experts valueable  suggestions ..........

 

Regards

ABDUL JABBAR KHAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...