Re: [MW:12012] Roller marks

Mr Navaneethakumar,

                  Please can you  give more details like design code,service condition. design temperature and pressure.

if the  service condition are   high pressure&temperature  then these are not acceptable..!!

if it is normal  pressure  and temperature depends on service condition you  can make your  judgement and accepted..!! 

simply rejecting is not a correct solution always !!!!


with regards,
sudhakar.k

On Sun, Jul 31, 2011 at 2:20 PM, navanee kumar <dnkuit@gmail.com> wrote:

Dear Experts,

Is it acceptable roller marks on the pipe?

Please find attached photographs.




 
Thanks&Regards,
Navaneethakumar.D.
+971505583738

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
With regards,
Sudhakar.k

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...