Sunday, July 31, 2011

Re: [MW:12008] FILLET WELD QUALIFICATION BY BUTT WELD AS PER API 1104

Mr.Islam ,
 
Your query is not correct ...5G position tells you that pipe is rotating but electrode is constant at 45 degrees
                                        2G position is tells you that pipe should be horizontal  position ..not in vertical ...
 
If the welder is qualified in buttwelds in limited thickness ...welder can qualify for all filletwelds ..unlimited thickness..
 
Thanks
 
Suresh
On Sun, Jul 31, 2011 at 2:09 PM, NAJM UL ISLAM <najmislam246@gmail.com> wrote:

Dear Experts,

Greetings,

 

Can somebody advise me that if a welder is qualified for butt weld either in 5G position (Pipe horizontal) or 2G position (Pipe Vertical) whether  he will be qualified for fillet welds or not.

 

Thanks & Regards

 

NAJM UL ISLAM

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.



--
Thanks  & Best Regards,

Suresh

Mobile No: 91-92 92 905 905

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...