Why gas purging is not mandatory for MIG welding as it is mostly used for TIG welding?

In MIG welding i found contamination is very lass as compared to TIG welding without purging.

Can any one clarify me??????


Regards
Prasad


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS