Manpreet,
Sec IX not in picture .
On Tue, Jul 26, 2011 at 10:32 AM, manpreet <manpreetsin88@rediffmail.com> wrote:
Hi,Unfortunately you can not use PQR (P1 Gr2 to P1 Gr2) to weld P1 Gr1 to P1 Gr2, find out if you have PQR qualified with P1 Gr1 to P1 Gr2.Intent of code is to have impact test done on both material else look for a material with dual certificate (both Gr1 & Gr2).RegardsManpreet SinghSent: Tue, 26 Jul 2011 07:53:34
Subject: [MW:11886] AWS D1.1 Table 4.6 Clause 1-Change in Group No.Treat yourself at a restaurant, spa, resort and much more with Rediff Deal ho jaye!Gents,WPS is qualified in Group II to Group II, with CVN @-40 deg. cel.,Can we use this WPS , to weld Group II to Group I combination with requirement of CVN @-20 deg cel.--
Thanks & regards,
K.Babu
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
--
Thanks & regards,
K.Babu
Singapore
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
Comments