Dear Navaneetha kumar,
 
It is not clear for what application the pipe is ?????????
 
If the pipe is for High Pressure line then it should be REJECTED.
 
Regards
 
Abdul Jabbar Khan

--- On Sun, 31/7/11, navanee kumar <dnkuit@gmail.com> wrote:

From: navanee kumar <dnkuit@gmail.com>
Subject: [MW:12001] Roller marks
To: materials-welding@googlegroups.com
Date: Sunday, 31 July, 2011, 2:20 PM


Dear Experts,

Is it acceptable roller marks on the pipe?

Please find attached photographs.




 
Thanks&Regards,
Navaneethakumar.D.
+971505583738

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...