Tuesday, July 26, 2011

Re: [MW:11930] FCAW for Duplex stainless steel

Try FSH( selectarc ) superduplex basic flux cored wire with Argon/co2 mix gas.
vanchi

On Sat, Jul 16, 2011 at 8:31 AM, 박종민(PARK, JONG MIN) <carpediem@dsme.co.kr> wrote:

Dear Experts

 

I wan to use FCAW process for welding of duplex stainless steel.

However, CVN value shall be min.50 Joule at -46 degree C.

Is there any flux cored wire which meets this requirement?

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...