Re: [MW:12005] Roller marks

Not acceptable

Regards
Mahmoud Qreis

On Jul 31, 2011, at 12:50 PM, navanee kumar <dnkuit@gmail.com> wrote:


Dear Experts,

Is it acceptable roller marks on the pipe?

Please find attached photographs.




 